Characterization Of Multi-layered Fish Scales (Atractosteus spatula) Using Nanoindentation, X-ray CT, FTIR, and SEM

14.9K Views

10:06 min

July 10th, 2014

DOI :

10.3791/51535-v

July 10th, 2014

14,903 Views

1Geotechnical and Structures Laboratory, U.S. Army Engineer Research and Development Center, 2Department of Mechanical Engineering, University of Alabama, 3Environmental Laboratory, U.S. Army Engineer Research and Development Center