1Department of Mechanical Engineering, Massachusetts Institute of Technology, 2Laboratory for Manufacturing and Productivity, Massachusetts Institute of Technology, 3School of Engineering and Applied Sciences, Harvard University, 4Department of Materials Science and Engineering, Massachusetts Institute of Technology, 5Department of Chemistry & Chemical Biology, Harvard University

Tin sulfide (SnS) is a candidate material for Earth-abundant, non-toxic solar cells. Here, we demonstrate the fabrication procedure of the SnS solar cells employing atomic layer deposition, which yields 4.36% certified power conversion efficiency, and thermal evaporation which yields 3.88%.

Tags

Ing nierie

-- Views

Related Videos

JoVE Logo

Privacy

Terms of Use

Policies

Research

Education

ABOUT JoVE

Copyright © 2024 MyJoVE Corporation. All rights reserved