Four-phase Indium Tin Oxide (ITO) Electrode Fabrication
3:00
Janus Particles Preparation
5:11
Metallic Particle Preparation
6:46
Alternative Current Electrokinetic Measurements
7:59
Results: EROT and DEP Measurements of Janus Particles and Fully-coated Metallic Particles
9:14
Conclusion
Transcript
The overall goal of this procedure is to rapidly fabricate indium tin oxide electrodes and prepare metal-coated particles for electrokinetic experiments. This method can facilitate experiment in electrokinetics field, such as electrorotation, diel
Sign in or start your free trial to access this content
In this article, a simple method to prepare partially or fully coated metallic particles and to perform AC electrokinetic property measurements with a rapidly fabricated indium tin oxide (ITO) electrode array is demonstrated.