Войдите в систему

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.

The integrity of the mortar joints can be preserved by using weather-resistant mortar and ensuring the mortar is well-filled in the joints and compacted adequately during bricklaying. In severe climates, even with these measures, mortar joints in masonry walls will exhibit considerable deterioration. In such conditions, deteriorated mortar joints must be repointed. Repointing involves removing deteriorated mortar by cutting, raking, and replacing it with new mortar. In the case of hairline cracks in mortar joints, surface grouting is done in the joints to preserve masonry walls' structural integrity and appearance.

Теги
Mortar Joint DeteriorationMasonry StructuresWater AccumulationFreeze thaw CyclesCracks PropagationSpallingMoisture IntrusionWeather resistant MortarBricklayingRepointingSurface GroutingStructural Integrity

Из главы 2:

article

Now Playing

2.12 : Mortar Joint Deterioration in Masonry

Masonry

86 Просмотры

article

2.1 : Composite Masonry Walls

Masonry

401 Просмотры

article

2.2 : Masonry Cavity Walls

Masonry

317 Просмотры

article

2.3 : Masonry Loadbearing Walls

Masonry

79 Просмотры

article

2.4 : Masonry Curtain Walls

Masonry

367 Просмотры

article

2.5 : Posttensioned Masonry Walls

Masonry

90 Просмотры

article

2.6 : Cavity Drainage and Flashings in Masonry walls

Masonry

56 Просмотры

article

2.7 : Thermal Insulation in Masonry Walls

Masonry

90 Просмотры

article

2.8 : Expansion and Contraction in Masonry Walls

Masonry

276 Просмотры

article

2.9 : Movement Joints in Buildings

Masonry

82 Просмотры

article

2.10 : Types of Building Separation Joints

Masonry

148 Просмотры

article

2.11 : Efflorescence in Masonry

Masonry

55 Просмотры

article

2.13 : Masonry in Cold and Hot Weather Conditions

Masonry

63 Просмотры

article

2.14 : Masonry Paving

Masonry

225 Просмотры

JoVE Logo

Исследования

Образование

О JoVE

Авторские права © 2025 MyJoVE Corporation. Все права защищены