Material Formation of Recombinant Spider Silks through Aqueous Solvation using Heat and Pressure

5.1K Views

10:26 min

May 6th, 2019

DOI :

10.3791/59318-v

May 6th, 2019


Trascrizione

Esplora Altri Video

Recombinant Spider Silk

Capitoli in questo video

0:04

Title

2:21

Recombinant Spider Silk Mixture Preparation from Lyophilized Protein Stocks

3:03

Recombinant Spider Silk Solvation

4:05

Hydrogels, Sponges, and Lyogel Preparation

4:55

Films, Coatings and Adhesives

6:01

Wet-Spun Fibers

9:04

Results: Aqueous Solvation and rSSp Materials

9:38

Conclusion

Video correlati

article

08:30

Visualizzazione del DNA ricombinante e Complessi proteina usando la microscopia a forza atomica

22.3K Views

article

13:36

Sintetico di produzione Spider Silk su scala di laboratorio

26.6K Views

article

10:11

Cella Co-cultura Patterning Uso acquose due sistemi monofase

18.3K Views

article

09:51

Filtro aria dispositivi tra cui maglie non tessuti di elettrofilate ricombinanti Spider Proteine ​​della Seta

16.0K Views

article

13:02

Microfabrication di Patterns Oro nanoporosi per Cell-materiali Interaction Studies

11.3K Views

article

07:19

Protocollo per il Biofilm Streamer formazione in un dispositivo a microfluidi con Micro-pilastri

12.1K Views

article

10:26

Photopatterning proteine ​​e cellule in acquosa ambiente utilizzando TiO

7.8K Views

article

06:50

Microambienti sandwich di sfruttare Cellulari / Materiale Interazioni

7.5K Views

article

11:51

Ingegneria fluorescenza 'D'oro' per incorporazione di pressione selettiva di aminoacidi Non canonico e l'analisi della proteina di fluorescenza e di spettrometria di massa

11.8K Views

article

11:12

Ottimizzazione di un'analisi di espressione di RNA-ha basato multisala usando materiale archivistico di cancro al seno

7.7K Views

JoVE Logo

Riservatezza

Condizioni di utilizzo

Politiche

Ricerca

Didattica

CHI SIAMO

Copyright © 2025 MyJoVE Corporation. Tutti i diritti riservati