Source: Laboratory of Dr. Terry Tritt — Clemson University
Differential Scanning Calorimetry (DSC) is a method of thermodynamic analysis based on heat-flux method, wherein a sample material (enclosed in a pan) and an empty reference pan are subjected to identical temperature conditions. The energy difference that is required to maintain both the pans at the same temperature, owing to the difference in the heat capacities of the sample and the reference pan, is recorded as a function of temperature. This energy released or absorbed is a measure of the enthalpy change (ΔΗ) of the sample with respect to the reference pan.
1. Baseline Measurement
ZnO formation via Decomposition of ZnCO3
The change in enthalpy per degree, at constant pressure is equivalent to the heat capacity of a material at constant pressure given by Equation 1. The enthalpy change is obtained by estimating the area under the curve between two temperature limits given by Equation 2.
(Equation 1)
A major application area of DSC is the glass transition (Tg) in amorphous polymers, in which the material changes from a rigid glassy state to a viscous liquid state. Pharmaceutical research on nano-particles is also an emerging field, where the DSC has been used to quantify amorphous or crystalline phase in nano-solids. A review of DSC techniques on applications in biology and nano-science has been provided by Gill et al.3 Nanostructured lipid carriers (NLC) have potential applications in
Przejdź do...
Filmy z tej kolekcji:
Now Playing
General Chemistry
44.8K Wyświetleń
General Chemistry
659.1K Wyświetleń
General Chemistry
275.4K Wyświetleń
General Chemistry
557.0K Wyświetleń
General Chemistry
383.9K Wyświetleń
General Chemistry
183.8K Wyświetleń
General Chemistry
141.6K Wyświetleń
General Chemistry
347.0K Wyświetleń
General Chemistry
425.8K Wyświetleń
General Chemistry
79.4K Wyświetleń
General Chemistry
158.9K Wyświetleń
General Chemistry
265.8K Wyświetleń
General Chemistry
160.8K Wyświetleń
General Chemistry
196.4K Wyświetleń
General Chemistry
91.8K Wyświetleń
Copyright © 2025 MyJoVE Corporation. Wszelkie prawa zastrzeżone